Tuesday

THE DETAILS OF A CONCRETE DELIVERY TICKET Understand what you’re signing when you accept concrete deliveries.

Editor’s Note: This is part one of a two-part article. Look for the second installment in the July issue.
Every load of ready-mixed concrete comes with a delivery ticket full of useful information, if you know how to crack the secret code. Critical information includes identifying the mix, batch, and cumulative volume; help on checking yield; admixtures; and the amount of water that can be added within specs. The ticket also tells the batch time, which is important for predicting slump loss and setting time, and there is a lot of important cost information that will help you figure out what the concrete is worth (if you are delivering it) or how much you will have to pay (if you are receiving it).
Besides of all of this, if and when something hits the fan on your concrete project, the tickets are likely to be introduced as evidence, marked “Exhibits A, B, and C.” But despite this practical and economic value, concrete delivery tickets “just don’t get no respect.” When I needed some fresh tickets for an upcoming presentation, I visited the nearest construction site and found three of them blowing away in the wind!

The right mix

If you have ever placed concrete only to find out that you put the wrong mix in the wrong place, you already know how important it is to check the mix ID on the ticket. Look for the customer and jobsite info, special delivery instructions (back gate, east entrance) and the mix ID. Most producers have an ID code such as “4012” for non-air-entrained 4000 psi (@ 28 days) with #1 and #2 stone, or perhaps “4012AE” for a similar air-entrained mix. Special features such as fibers will often be in the mix designation as well.
Of course the busiest time onsite is when you are trying to get a pour started, which is when the concrete is being delivered. But if you don’t have the time to read the ticket to make sure that you are about to place the right mix, you have to ask yourself, “Do you have time later to deal with having placed the wrong mix?” If you only have one mix on the project, and your producer is shipping to you only, this may not be a big deal. But if you have a footing mix, slab-on-ground mix, column mix, and elevated-slab mix, and if your job is big enough that any of these can be placed on a given day, it pays to check the ticket.
The ticket also shows the volume of concrete in this load, and the total volume of the same mix shipped for this order today. It is important to know that these are calculated volumes, not measured volumes (more on yield later). This total cumulative volume is essential for managing your concrete order. Given the unevenness of subgrade, variable slab thickness, deformation of forms, settlement of shoring, and variable air content and yield of the concrete, it is tough to predict the exact volume of concrete to order. One common routine is to give the concrete producer an estimated total volume (say 100 cubic yards) and a hold value (maybe 96 cubic yards). But the trick is to make your final order before that last truck arrives. At the end of any given load, say 80 or 88 cubic yards, you can check the ticket, discover total yardage placed, estimate the volume to complete (maybe add ½ yard), and call in your final order.

he sales receipt

On smaller jobs the ticket serves as the only purchase order or sales agreement between the contractor and the producer. For that reason, it is common for the ticket to show price per cubic yard and total price per load. Extra charges may appear for items such as hot water in cold weather, extra cost for a partial load, or for long unloading times (overtime). It is common for the ticket to include text that describes these charges, and reading these terms and noting extra charges can reduce “sticker-shock” when the invoice shows up in the mail, because unless you are familiar with the terms under which the concrete was purchased, that invoice with all its extras can remind you of a cellphone bill or a rental car receipt.
For example, in the “mock-up” delivery ticket shown on page 21, the fine print indicates a split-load charge for orders less than 4 CY. This recognizes that the price structure for ready-mixed concrete includes the variable cost of the materials and the prorated cost of transport, plant and equipment, and driver. For small orders, the split-load charge helps to fairly cover these fixed costs.
Similarly, the concrete producer assumes a typical time onsite to discharge the concrete; five minutes per yard in our example. This also relates to the per-cubic-yard pricing of ready-mixed concrete by accounting for driver time and overall per cubic yard productivity. The example ticket indicates that the total discharge time recorded by the driver (and approved by the customer who signed the ticket) exceeded the allocated five minutes per CY. This overtime was charged at the rate announced in the fine print of $75 per hour.
Along with the printed “terms and conditions,” you are likely to find material safety data information along with statements that limit the producer’s responsibility for the finished product, given that control of the product passes to the contractor at the end of the chute. While it is common for an employee of the contractor to hastily scribble initials on the ticket when done with the truck, if you look closely that representative may have signed that he or she “inspected, approved, and received” the concrete. Those words make the scribbled signature more important than usually realized.

Slump loss and setting time

The ticket itself is a serial-numbered document to distinguish it from all others ever printed by that concrete producer. It will show the truck number, perhaps the driver’s name, and the date and time of batching. This is essential because most specs require that concrete may be discharged from the truck only up to 90 minutes (or sometimes less) after the batch time. Tickets may also show the times at which the truck left the plant, arrived onsite, began to discharge, and completed discharge. This information can be used to check spec compliance, as mentioned, determine any overtime truck charges, or to help explain or predict rate of slump loss or setting times.
Complaints from contractors about apparent truck-to-truck variability in slump, rate of slump loss, or setting time are not uncommon. But these characteristics are tied to the rate of hydration of the cement, temperature of the concrete, and the time at which cement and water first came into contact. Slump-loss and setting begin at batch time (printed on the ticket), but the contractor (or finisher on the deck) is far more aware of the time at which the concrete was placed.
For example, let’s say the first truck beat morning traffic and got to the site 15 minutes after batching, but the second truck carrying identical concrete had a 30-minute haul time. The second truck is likely to arrive at a lower slump, and is likely to appear to have a setting time 15 minutes shorter than the first. In cool weather this might not matter, but under hot, dry, sunny, or windy conditions, those might be 15 very important minutes. Of course, any actual batch-to-batch variation in slump or setting will just add to variable time-since-batching, but important clues are right there on the truck ticket.
This is demonstrated with the setting time data shown on the graphs at left. Using a variation on the ASTM C403 test, the pressure required to embed a boot-sized footprint into fresh concrete to a depth of ¼ inch is measured. This pressure is shown on the vertical axis. For this field test of concrete paving at a mall, the finishers could float the concrete when the penetration resistance was about 5 psi, and could apply the appropriate broom finish when the penetration resistance was about 15 psi. In the top graph, the horizontal axis shows time after placing the concrete, with about an hour difference in float-time between truck 60 and truck 28. The bottom graph shows that there was only about a 15-minute variation in batch-to-batch setting when time is measured from batch time instead of placing time. Note that the first truck of the day, #167, was clearly a load of slower-setting concrete anyway you measure it!
The information discussed so far constitutes what is known as the Delivery Ticket, and is not significantly different from the receipt that accompanies delivery of many other construction materials. The second article in the series will explore the Batch Ticket with its details of concrete mixture composition, often printed on the same piece of paper. As we will see, ASTM C94, Standard Specification for Ready-Mixed Concrete, makes it clear that detailed batch information must be provided only when specified. Inclusion of such data is therefore not automatically mandatory.

Monday

Deterioration of Concrete Structures

Why concrete structures fail? Concrete has long been known as a reliable construction material, but deficiencies in material selection, detailing, and design can affect the service life of Concrete. Deterioration of concrete structures can become a challenge for the owners of these structures. It is important to identify these defects on time, and plan appropriate repair strategies. In this article, we will review some of the most famous deterioration mechanisms. In doing so, we have focused on the Ontario Structure Inspection Manual (OSIM, 2008). In addition, the review of the following two documents is highly recommended in learning defects and deterioration of concrete (Reference 1 and Reference 2).

Deterioration of Concrete

Before we begin this review, It is good to review the definition of the following two terms according to the OSIM (2008):

Defect: An identifiable, unwanted condition that was not part of the original intent of design.
Deterioration: A Defect that has occurred over a period of time

Different defects can be involved in the deterioration of concrete.  The following review provides a brief summary on the most common defects observed in the existing structures. Normally, one or a number of these defects can be seen in structures; therefore, it is necessary to identify them properly. One needs to understand these different defects properly in order to get more realistic evaluation of the structure.

1- SCALING

What is it?

Scaling is referred to the loss of the surface portion of concrete (or mortar) as a result of the freezing and thawing (OSIM, 2008). It is a physical action that usually leaves the aggregates clearly exposed. (PCA, 2001).

How it happens?

Scaling happens when the hydraulic pressure from water freezing within concrete exceeds the tensile strength of concrete. Scaling is more common in non-air-entrained concrete, but can also occur in air-entrained concrete in the fully saturated condition.

2- DISINTEGRATION

What is it?

Disintegration is the physical deterioration (such as scaling) or breaking down of the concrete into small fragments or particles.

How it happens?

It usually starts in the form of scaling. It may be also caused by de-icing chemicals, sulphates, chlorides or by frost action.

3- EROSION

What is it?

Erosion is the deterioration of concrete surface as a result of particles in moving water scrubbing the surface.

How it happens?

When concrete surface is exposed to the water-borne sand and gravel, the surface gets deteriorated by particles scrubbing against the surfaces. Flowing ice particles can also cause the problem. It is an indicator of poor durability of concrete for that specific exposure.

4- CORROSION OF REINFORCEMENT

What is it?

Corrosion is the deterioration of steel reinforcement in concrete. Corrosion can be induced by chloride or carbonation. The corrosion can result in cracking in the concrete cover, delamination in concrete decks, etc.

How it happens?

When the concentration of chloride ions above the surface of reinforcement reaches the threshold limit (which is the amount required to break down the passive film) corrosion begins. The volume of resulting material (rust) is 6-7 times, which increases the stress around the rebar, and causes fracture and cracking. The cracks extend to the surface of concrete over time; that is when we can visually see the sign of rust over the surface of concrete.  

Learn More: Structural Effects of Corrosion


5- DELAMINATION

What is it?

“Delamination is defined as a discontinuity of the surface concrete which is substantially separated but not completely detached from concrete below or above it.” (OSIM, 2008). Delamination is often identified by the hollow sound by tapping or chain dragging of concrete surface.

How it happens?

The corrosion of reinforcement and subsequent cracking of the cover can cause delamination. When the rebar have small spacing, the cracking extends in the plane of the reinforcement parallel to the exterior surface of the concrete.

6- SPALLING

What is it?

Spalling can be considered an extended delamination. In fact, when the delamination continues, the concrete fragments detach from a larger concrete mass.

How it happens?

If delamination is not repaired on time, the progress of damages as a result of external loads, corrosion, and freezing and thawing can break off the delaminated pieces.

7- ALKALI-AGGREGATE REACTIONS

What is it?

It is the internal cracking of concrete mass as a result of a chemical reaction between alkalis in the cement and silica in the aggregates. The AAR/ASR cracking are very famous for their crack patterns.

How it happens?

The alkalis in the cement can react with the active silica in the aggregates to form a swelling gel. When this gel absorbs water, it expands, and applies pressure to surrounding environment which makes the concrete crack.

8- CRACKING OF CONCRETE

What is it?

A crack is a linear fracture in concrete which extends partly or completely through the member.

How it happens?

Some people believe that concrete is born with cracks; that its ingredients, and how it is produced - from the batching plant to pouring, setting, and curing - is influenced by so many factors that cracking of concrete does not come as a big surprise; and to a great extent, that might be true. Cracking of concrete can happen in different stages: It can happen before hardening of concrete, and it can happen in an old concrete structure:

Before Hardening

+ Settlement within concrete mass
+ Plastic shrinkage

After Hardening

+ Drying shrinkage
+ Thermal contraction
+ Sub-grade settlement

Sunday

Non-Destructive Evaluation of Unknown Foundations

Non-destructive evaluation of unknown foundationsand piles has gained interest among engineers and researcher over the past few years. Latest research show the effectiveness of these methods in investigating the depth and quality of existing piles, as well as in the quality assurance of new construction.
Piles are structural members made of timber, steel, or concrete. Piles are used to transfer the loads of a heavy superstructure (bridge, high rise building, etc.) to the lower layers of soil.
In the design process, estimating the unknown length of piles and drilled shafts is an important challenge; this remains true for verification and quality assurance of newly constructed foundation. Evaluating the integrity and length of existing piles is another important issue in the assessment of quality and performance of piles. Testing existing piles can be quite challenging as these elements are embedded in the ground, with limited and sometimes impossible access. This is specially true if structural drawings and documentations are missing.

Non-Destructive Evaluation of Unknown Foundations

Non-Destructive Testing (NDT) methods provide an excellent tool for evaluating the length and integrity of existing piles. Different NDT methods have been developed and tested within the past two decades. A comprehensive study performed by the Bridge Maintenance Office of the Florida Department of Transportation and FHWA investigates and researches testing methods for a cost effective and accurate evaluation of potential risks. As part of this research, the most current and widely used non-destructive testing (NDT) methods for determining the embedment depth of bridge foundations were identified.

Existing NDT Methods

Two general categories of NDT testing is used in evaluating the length of piles:

1- Surface NDT Methods

Surface NDT methods do not require any soil boring or probe. The main advantage with this group is that they are typically fast, with minimal intrusion. The equipment can easily be moved around the top of the substructure. The traffic disruption caused by this group of tests is often minimal. A major disadvantage to surface NDT are its inability to provide foundation data below a subsurface pile cap (if one exists).
+   Pile Integrity Test (PIT)
+   Bending Waves with Short Kernel
+   Ultra-Seismic
+   Surface Wave Spectral Analysis
+   Ground Penetrating Radar
+   Dynamic Foundation Response

2- Subsurface NDT

Subsurface NDT methods require the installation of at least one soil boring or probe. A big advantage of this group of tests is their ability to detect foundations below a subsurface pile cap. One drawback for this group of tests is the fact that they are often more expensive. However, this can be justified by the greater reliability and versatility they offer.
+   Parallel Seismic
+   Borehole Radar
+   Borehole Sonic
+   Cross Hole Sonic
+   Induction Field
+   Borehole Magnetic

How to Choose the Right Test?

The selection of proper NDT method comes to the question of accessibilitytraffic, and the top part of the substructure, that is whether the piles have cap or not. One should also consider the following when making a decision:
+   Pile material
+   Pile configurations in the foundation layout
+   Pile surrounding area (material)
+   Pile condition (exposed or covered up by pile cap)
+   Ground water level


How to Perform Pile Integrity Test

Concrete piles and drilled shafts are an important category of foundations. Despite their relatively high cost, they become necessary when we want to transfer the loads of a a heavy superstructure (bridge, high rise building, etc.) to the lower layers of soil. Pile integrity test (PIT), or as ASTM D5882 refers to it as low strain impact integrity test, is a common non-destructive test method for the evaluation of pile integrity and/or pile length. Pile integrity test can be either used for for forensic evaluations on existing piles, or quality assurance in the new construction. The integrity test is applicable to driven concrete piles and cast-in-place piles.

Low strain impact integrity testing provides acceleration or velocity and force (optional) data on slender structural elements (ASTM D5882). Sonic Echo (SE) and Impulse Response (IR) are employed for the integrity test on deep foundation and piles. The test results can be used for evaluation of the pile cross-sectional area and length, the pile integrity and continuity, as well as consistency of the pile material; It is noted that this evaluation practice is approximate.
The PIT method works best for column type foundations, such as piles and drilled shafts. The method provides a rapid and simple tool for evaluation of a number of piles in a single working day.

How to Perform PIT?

The pile head surface should be accessible, above water, and clean of loose concrete, soil or other foreign materials resulting from construction. Any type of contamination should be removed (using a grinder) to reach to solid and sound concrete surface. This step is so vital, because then connection between the sensor and concrete should be solid (firm contact). The location of the sensor should be selected away from the edges of the pile. The integrity testing should be performed no sooner than 7 days after casting or after concrete strength achieves at least 3/4 of its design strength, whichever occurs earlier.
A hammer (with or without force measurement unit) is used for impacting pile top; the impact should be applied axially with the pile. Motion transducer should be capable of detecting and recording the reflected echos over the pile top. Acceleration, velocity, or displacement transducers can be used for this purpose. At the minimum, acceleration transducer should have an Analog to Digital Converter with 12 bit resolution; and a Sample Frequency of at least 25 KHz.
The distance between the impact location and the sensor should be no larger than 300 mm. Several impacts are applied to the top of the pile. The reflected echos are then recorded for each individual impact. As an alternative, the average can be determined and used. As mentioned earlier, acceleration transducer can be used for the purpose of this test. In this case, the apparatus shall provide signal conditioning and integrate acceleration to obtain velocity. The apparatus shall balance the velocity signal to zero between impact events.

What Information Does Pile Integrity Test Provide?

The Pile Integrity Test (PIT) provides information about:
+ Continuity of pile
+ Defects such as cracks
+ Necking
+ Soil incursions
+ Changes in cross section
+ Approximate pile lengths (unless the pile is very long or the skin friction is too high).

Limitations of Pile Integrity Test

The PIT provide an indication of soundness of concrete; however, the test has certain limitations:
+ PIT can not be used over pile caps.
+ It does not provide information regarding the pile bearing capacity.
+ Test should be undertaken by persons experienced in the method and capable of interpreting the results with specific regard to piling.
+ This test is not effective in piles with highly variable cross sections
+ It is not effective in evaluating sections of piles below cracks that crosses the entire cross sectional area of the pile.
The primary shock wave which travels down the length of the shaft is reflected from the toe by change in density between the concrete and the substrata. However, if the pile has any defects or discontinuities within its length these will set up secondary reflections which will be added to the return signal.

Saturday

5 Tips for Hot Weather Concreting

Extreme weather conditions (extreme heat or cold, and humidity variations) can significantly alter the quality of concrete. In hot weather concreting, one should make sure that all the negative impacts of high ambient temperature are appropriately alleviated by taking the necessary precautions. In this article, we will review how hot weathertemperatures can affect the quality of concrete construction. We will also review some of the most important precautions for concreting during the hot season.

What is Hot Weather for Concreting?

Let’s see what hot temperature is for concrete, and why it is critical. American Concrete Institute (ACI) definition of hot weather condition, as stated in the ACI-305R-10, refers to job-site conditions that accelerate the rate of moisture loss or rate of cement hydration of freshly mixed concrete, including:
   a)  Ambient temperature of 27 °C (80°F) or higher; and
   b)  Evaporation rate that exceeds 1 kg/m2/hCanadian Concrete Design code (CSA A23.1/.2) uses the same ambient temperature for hot weather (27 °C).

Challenges of Hot Weather Concreting

How does hot temperature affect concrete? We know that water is a main component in concrete. Increase in the weather temperature increases the rate of vaporization, therefore, hot weather condition increases the water demand in concrete production.  Other challenges of hot weather concreting can be summarized as:
1- Accelerated slump loss leading to the addition of water on the job-site,
2- Increased rate of Setting resulting in placing and finishing difficulties,
3- Increased tendency for thermal and plastic cracking,
4- Critical need for prompt early curing,
5- Difficulties in controlling entrained air,
6- Increased concrete temperature resulting in long term strength loss.

Precautions for Hot Weather Concreting

Following general precautions will help in performing a successful concreting project in hot weather conditions, and mitigating the negative impacts of hot weather. These precautions would be helpful during concrete production and delivery, and will improve the durability performance of concrete by minimizing undesired cracking.
1- Use materials and mix proportions that have a good record in hot-weather conditions,
2- Cool the concrete or one or more of its ingredients,
3- Use a concrete consistency that allows rapid placement and consolidation,
4- Reduce the time of transport, placing and finishing as much as possible,
5- Schedule concrete placements to limit exposure to atmospheric conditions (i.e. at night or during favorable weather conditions).

General Solutions for Cooling Materials

The usual method of cooling concrete is to lower the temperature of the concrete materials before mixing. The aggregates and mixing water should be kept as cool as feasible as these materials have a greater influence on concrete temperature after mixing than other ingredients. In extreme hot condition, a portion of water can be replaced with ice to lower the temperature. Curing of concrete plays a significant role in reducing the negative impacts of hot weather on the quality of concrete.

Corrosion Monitoring of Reinforced Concrete Structures

A corroded structure (whether it is a bridge, or a jetty, or a simple ramp) could be scary for many people. Imagine yourself driving along the Gardner Express (Downtown Toronto), or the highway 40 (Montreal), and all of a sudden, a piece of concrete falls onto your car, breaking the windshield. Feels scary? Indeed! A corroded structure makes you feel so unsafe, even if it is in stable condition. This makes the corrosion investigation of bridges a very important task in the asset management process.
Corrosion monitoring of reinforced concrete structures can be quite challenging. It is hard to detect corrosion at the early stages; On the other hand, it is almost too late when we can see the corrosion signs on the surface. Detecting corrosion in a concrete structure require appropriate knowledge, proper inspection tools and experience. Many structural engineers ask what is the best practice in corrosion investigation? Some want to know where to start their search? Others are concerned about the accuracy, and precision of available test methods, and some others want to know if the results of such investigation is of any use from structural engineering perspective!

Corrosion Monitoring of Reinforced Concrete Structures

Corrosion monitoring could be quite challenging. A proper test plan should take into account the following considerations:
1- Exposure condition (Access to moisture, oxygen, exposed to de-icing salts, other chemicals, carbon dioxide);
2- Geometry of the structures and components;
3- Access to structural and non-structural components;
4- Dimension and scale of the area under investigation;
5- Importance of the element, etc.
A careful review of the exposure condition can also help in selecting the best monitoring techniques and tools.
Lets take a bridge structure. A bridge has so many components: deck, piers, girders, abutments, expansion joints, etc. Depending on which element is being inspected, the inspection method could vary. For example, chain dragging and half-cell potential mapping is widely used for bridge deck scanning; However, prestressed girders (specially those in the middle) need to be inspected using more comprehensive techniques for identifying and locating corrosion of prestressing tendons. The following inspection procedures are widely used during  a routine corrosion monitoring program:

Chain Drag Delamination Survey

Chain dragging is widely used to detect delamination in concrete bridge decks. The concept behind this very simple method is the unique hollow sound that is made by dragging chain across the delaminated surface. The test is used to identify potentially delaminated areas on the deck slab.
The main advantage of the method is that it is very simple, and no special equipment is required. However, chain dragging in the field needs some training. The practice is difficult when vehicles are moving over the deck, and distinguishing the hollow sound becomes difficult.
The main disadvantage of the chain dragging method is that they can only provide results if the defect and deterioration are in well advanced stages. Early diagnosis of damage mechanism is not possible using this technique. Application of the method is somewhat difficult during heavy traffic.

Chloride Content (Profile)

Measuring the chloride content in concrete cover (and at the rebar surface) is a classic method in corrosion investigation of concrete structures. Powder samples are obtained from different depths (usually 5 depths from exposed surface to rebar level), and chloride profile is developed. Diffusion coefficient can be determined in this method. The main advantage is to understand if the concentration of chloride ion is higher than the threshold value (the amount required for depassivating the protective film over rebar).

Electrical Resistivity Measurement

The use of electrical resistivity method for quality control and evaluation of concrete durability is becoming very popular among scholars and engineers. The measurement of electrical resistivity of concrete provides useful information about the microstructure of concrete material. The test procedure has since been standardized by AASHTO TP 95.
This method is adapted by several Department of Transportation (DOTs) to replace the labour-intensive and time-consuming methods such as the ASTM C 1202, “Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration”, generally known as the Rapid Chloride Permeability Test (RCPT). The application of electrical resistivity measurement for scanning concrete deck was studies in studied as part of a research program (read more).
Electrical resistivity measurement is easy and fast to perform over concrete bridge deck; It can provide useful information about the resistance of concrete material to penetration of chloride ion. Electrical resistivity measurements are effected by moisture content, salt content of concrete, and presence of steel rebar. This makes the task of data interpretation difficult.

Half-Cell Corrosion Potential Mapping

Half Cell corrosion mapping offers a rapid, cost-effective and non-destructive way for corrosion assessment. The test provides valuable information on the likelihood of corrosion, and helps in the quality assurance of concrete repair and rehabilitation. Several standard associations have standardized the test procedure including the ASTM C 876UNI 10174 and RILEM TC 154. Depending on the measured half cell corrosion potential value, the probability of active corrosion is determined. 

Corrosion Rate Measurement

Half-cell potentials do not provide any information on the kinetics of the reactions. Why is that important? The kinetics can help us predict how fast reinforcing bars are corroding. This can help predict the remaining service life of a structure, and help prepare a comprehensive maintenance plan. Several techniques are available for measuring the corrosion rate. Most of them rely on predicting the polarization resistance of reinforcement. Conventional test methods require a connection to reinforcement mesh; recent developments in the industry offer connection-less methods, which makes it faster, and less intrusive.

Ground Penetrating Radar - GPR

GPR is mainly used for sub-surface imaging of concrete decks. However, with the recent developments in the radar technology, the technique is now being used for corrosion monitoring as well. The ease of use, and the fact that scanning can be performed at the highway speed makes this method particularly important for large bridge decks. However, using GPR for corrosion monitoring needs trained and experienced individuals.
GPR uses electromagnetic radiation in microwave band of the radio spectrum, emitting radar pulse into the medium and detecting the reflected signals from subsurface media. A superposition of reflected signals is used to image the subsurface area. GPR is more accurate and robust to monitor the post-corrosion-initiation signs and side effects. It is obvious that GPR is not effective to monitor the corrosion signs at early stages.

AddToAny